Views: 0 Author: Site Editor Publish Time: 2026-11-18 Origin: Site
Driven by the ' dual carbon ' strategy, the low-carbon transformation of global chemical raw materials, and the continued tightening of environmental regulations, traditional petroleum-based synthetic additives and inorganic nanofillers have gradually shown shortcomings in many high-end scenarios: synthetic thickeners often have insufficient water resistance and aging resistance; inorganic fillers such as fumed silica and montmorillonite have high density and high carbon footprint, and are prone to forming stress concentration points in the resin matrix; small molecule emulsifiers migrate and precipitate, damaging the coating interface and barrier properties in the long term. The market urgently needs a new type of material that is renewable, has low environmental load, and has multiple functions of nano-reinforcement, rheology control, and interface stabilization.
Nanocellulose is a one-dimensional nanobiomass material prepared from natural cellulose through a top-down dissociation process. It is currently one of the categories with the fastest industrialization progress and the richest application scenarios in the field of bio-based nanomaterials cellulose nanofibers ( . According to the crystal morphology, preparation process and structural characteristics, mainstream products are divided into three categories: Among them, CNF , also often called MFC microfibrillated cellulose), cellulose nanocrystals ( CNC ), and bacterial cellulose ( BNC ). CNF and CNC are the mainstream of industrial supply. The structural difference between the two directly determines their adaptation logic in coatings and polymer composite systems: CNF is a continuous filament with a very high aspect ratio, relying on fiber entanglement to build a three-dimensional network, with outstanding advantages in rheology regulation, thickening, and toughness reinforcement; CNC is a short rod-shaped rigid crystal obtained by acid hydrolysis, with high crystallinity and stable elastic modulus. It is suitable as a rigid reinforcement phase to improve modulus, hardness and dimensional stability; BNC is produced by microbial fermentation and has extremely high purity and no lignin or hemicellulose impurities. However, due to production capacity and cost constraints, it is mostly used in high-end medical and special membrane materials, and is rarely used in the fields of large-scale coatings and modified plastics.
The raw materials of nanocellulose come from a wide range of sources, including bleached wood pulp, bamboo pulp, cotton pulp, straw, bagasse and other agricultural and forestry residual biomass. The raw materials themselves are carbon sequestration resources. The materials can biodegrade in the natural environment at the end of the life cycle, which is different from non-degradable petroleum-based polymers and inorganic fillers. However, the surface of native nanocellulose is rich in hydroxyl groups, and strong hydrogen bonding brings about two core contradictions: first, the drying process is easy to cause irreversible aggregation and is difficult to redisperse; second, the strong hydrophilic property makes it poorly compatible in non-polar resins and solvent-based systems. Without interface control, the addition will cause abnormal viscosity of the system, paint film defects, and mechanical property attenuation. Therefore, surface modification and dispersion processes are the core technical threshold for whether nanocellulose can be implemented in coatings and polymer composite materials.。
Ordinary cellulose is a micron-scale fiber bundle. The interior of the cellulose molecular chain relies on intramolecular hydrogen bonds to maintain stability, and the fiber bundles rely on intermolecular hydrogen bonds to tightly combine. The essence of nanocellulose preparation is to break the hydrogen bonds between fiber bundles and dissociate the fibers to the nanometer scale while retaining the structure of the cellulose molecular chain as much as possible.
· The theoretical elastic modulus of cellulose molecular chains can reach 130-150 GPa , which is much higher than that of most general-purpose polymers. At the same time, the density is only about 1.5 g/cm³ , achieving low density and ultra-high specific strength , and is an ideal base unit for lightweight reinforcement;
· The nanoscale brings extremely high specific surface area, up to 100-300 m²/g , and the surface is rich in hydroxyl active sites, providing sufficient reaction sites for chemical grafting and physical coating modification;
· In an aqueous dispersion system, nanofibrils form a reversible physical network through hydrogen bonding and hydrodynamics, showing typical thixotropic and shear thinning behaviors: the network maintains the viscosity of the system in a static state to prevent settling and sagging; when subjected to shearing (stirring, spraying, roller coating), the network temporarily dissociates, and the viscosity decreases to ensure construction leveling. After shearing is cancelled, the network is quickly rebuilt, which is its most unique rheological feature that distinguishes it from traditional thickeners.
Many downstream formulation developers tend to simply understand nanocellulose as ' green thickening powder ' , which is a simplified understanding of its mechanism of action. In coatings and composite material systems, its functions are divided into four independent and coordinated mechanisms:
1. Stress transfer and crack passivation mechanism (reinforcement) When nanocellulose achieves uniform dispersion of single fibrils in the matrix, the interface between the fiber and the resin forms an effective combination. Under the action of external force, stress can be transferred from the lower modulus polymer matrix to the high modulus nanofibrils. When microcracks occur inside the matrix, nanofibers can bridge the cracks, prevent further crack expansion, and change the fracture mode from brittle fracture to ductile fracture, ultimately improving the tensile strength, impact strength, wear and scratch resistance of paint films and composite materials. This mechanism is highly dependent on interfacial bonding. The interface of unmodified CNF in hydrophobic resin is weak, and it is easy for ' filling but not reinforcement ' or even performance degradation to occur.
2. Three-dimensional network barrier mechanism (barrier, anti-sedimentation) Evenly dispersed nanofibrils overlap each other to form a continuous and dense labyrinth network, extending the diffusion path of water vapor, oxygen, and corrosive media inside the coating, reducing the penetration rate, and improving the barrier performance of anti-corrosion coatings and packaging barrier coatings. At the same time, the network can wrap the inorganic pigment and filler particles in the system, reduce the free sedimentation rate of the particles, reduce stratification and precipitation, and improve the storage stability of the paint.
3. Interface adsorption stabilization mechanism ( Pickering emulsification) Nanocellulose is a solid particle emulsifier that can be adsorbed at - the oil-water two-phase interface. It relies on the steric hindrance and electrostatic repulsion of the particles themselves to stabilize the emulsion, replacing traditional small molecule emulsifiers. Small molecule emulsifiers have a small molecular weight and can easily migrate to the coating surface, causing poor water resistance, blistering, and loss of gloss. Nanocellulose particles are fixed at the interface and are not easy to migrate and have better long-term stability. They are an important technical route for low- VOC environmentally friendly emulsions and water-based functional coatings.
4. Film-forming and densification mechanism Nanocellulose itself has good film-forming ability. After drying, the fibrils are closely stacked to form a non-porous or less-porous film. When compounded with resin, it can fill the micropores generated during the resin curing process, reduce the porosity of the paint film, and further improve the solvent and boiling resistance.
Native nanocellulose is highly hydrophilic and is only suitable for fully aqueous systems; for solvent-based, solvent-free, polyolefin, epoxy, polyurethane and other hydrophobic matrices, surface modification must be carried out. The core goals of modification are to regulate surface energy, reduce hydrogen bond agglomeration, and improve interfacial compatibility with resins . The mainstream routes in the industry are divided into two categories: physical modification and chemical modification:
Grafting hydrophobic groups on the cellulose molecular chain through the chemical reaction of hydroxyl groups is the most stable solution for high-end composite materials and solvent-based coatings.
· Esterification modification: acetylation, maleation, stearoylation, etc., introducing long-chain alkyl groups, significantly reducing surface polarity, and can be dispersed in weakly polar solvents and polyolefin systems;
· Etherification modification: carboxymethylation and hydroxypropylation are mostly used to fine-tune the rheology of hydrophilic systems and are also the most mature pretreatment methods in industry;
· Silane coupling agent grafting: One end of the silane group reacts with the hydroxyl group of cellulose, and the other end is matched with epoxy, acrylic, and polyurethane resin. It is a very widely used modification scheme in the coating industry, taking into account both cost and interface effect. The advantage of covalent modification is that the modification effect is long-lasting and is not affected by solvents and pH . The disadvantage is that process control is difficult. Excessive modification will destroy the crystal structure of cellulose, loss of modulus and reinforcing effect, and the degree of substitution needs to be strictly controlled.
Using polymers, surfactants, and nanoparticles to adsorb and coat the surface of nanocellulose to change the surface properties, the process is simple and the cost is lower, and it is suitable for water-based coatings and emulsion systems. Commonly used coating agents include anionic polyacrylates, nonionic polymer dispersants, etc. This route will not destroy the cellulose crystal structure and retain the mechanical properties; the shortcoming is that the bonding force is weak. In high temperature and strong solvent environments, the coating layer is easy to desorb and the system stability is reduced.
Pre-dispersed nanocellulose is added directly during the resin polymerization process and relies on monomer polymerization to achieve in-situ infiltration. It is often used in thermosetting resin systems to minimize the problem of secondary dispersion and agglomeration in the later stage. It is suitable for small laboratory trials and high-end customized materials, but is difficult to produce continuously.
After the modification is completed, the product form will also be differentiated according to customer needs: low solid suspension, concentrated slurry, and redispersible powder. Concentrated slurry is currently the most popular choice for coating customers, balancing transportation costs and re-dispersion difficulty; powder products have the lowest transportation costs, but have strict requirements on dispersing equipment and dispersing processes. Many downstream factories lack high-energy dispersing equipment and are prone to the risk of agglomeration.
In water-based systems, low substitution degree modified CNF can be directly used to replace some polyurethane thickeners and alkali swelling thickeners. Compared with traditional thickeners, nanocellulose brings a wider thixotropic platform, lower high-shear viscosity, better spray leveling, higher low-shear viscosity, and stronger anti-settling ability of storage tanks. In the anti-corrosion primer, it is combined with anti-rust pigments such as zinc powder and zinc phosphate. The nano network improves the density of the paint film, reduces the penetration of water and chloride ions, and increases the duration of salt spray. In the wood varnish, it improves the hardness and wear resistance of the paint film, reduces sag during brushing, and reduces the overall VOC of the formula . It should be noted that the addition window is usually very low, and the addition amount of most systems is in the range of 0.2–1.5 wt% . Excessive addition can easily cause viscosity to soar and leveling to deteriorate. The formula needs to be rematched with dispersant, pH , and defoaming system.
Use CNF/CNC as the sole or compound emulsifier to prepare acrylic emulsion and water-based epoxy resin emulsion. The system does not add or significantly reduces small molecule emulsifiers. After curing, the coating's water resistance, humidity and heat resistance, and aging resistance are significantly improved. It is suitable for food contact packaging coatings, interior wall odor-free coatings, medical protective coatings, and other scenarios where precipitated substances are strictly restricted. This direction has been a research hotspot in recent years, but the difficulty lies in the control of the particle size of the emulsified particles and the stability of the emulsion against electrolytes. of nanocellulose . There are strict requirements for the zeta potential and dispersed particle size
PLA 、PBAT is the most mature degradable plastic on the market, but it has its own pain points of insufficient toughness, low heat deformation temperature, and poor dimensional stability. CNC serves as the rigid reinforcing phase and CNF serves as the tough network phase. When used in combination, the tensile modulus and impact strength can be improved at a lower addition amount, and the processing rheological properties can be controlled at the same time. The technical difficulty here lies in the thermal processing temperature: PLA processing temperature is usually 160-190°C . Nanocellulose is easily thermally degraded under aerobic high temperatures, causing yellowing of the material and mechanical decline. Therefore, nanocellulose used in degradable plastics generally needs to be equipped with thermal stability modification, or use a masterbatch blending process to shorten the high temperature residence time.
Hydrophobic modified CNF and acetylated CNC can be dispersed in epoxy resin and polyurethane matrix and used in lightweight composite materials composed of glass fiber / carbon fiber. Nanocellulose fills the gaps between glass fibers, reduces micropores inside the matrix, improves - the interfacial bonding of glass fiber resins, and increases interlayer shear strength. It is used for lightweight tooling, new energy structural parts, and functional panels. This type of scenario does not pursue extremely high additive amounts. The core value is to improve the fatigue performance and moisture and heat resistance of composite materials without significantly increasing density.
Although the academic literature on nanocellulose is very rich, in the process of large-scale implementation, a large number of customers will encounter the problem of ' excellent small-scale test results, loss of stability in pilot tests and mass production . ' The pain points are concentrated in four aspects:
1. Agglomeration problem : The hydrogen bonds of native fibers are extremely strong, and hard agglomerations cannot be broken up after drying; the dispersion process does not match, simple stirring cannot unravel the fiber bundles, and the agglomeration points become the source of pinholes, black spots, and mechanical defects in the paint film;
2. Batch consistency : There are batch differences in the biomass raw materials themselves. Small fluctuations in the dissociation process will cause fluctuations in aspect ratio, particle size distribution, and zeta potential, which directly affect the viscosity and reinforcing effect of the formula;
3. Poor process adaptability : Many downstream customers do not have high-pressure homogenization, micro-jet and other high-shear dispersion equipment, and cannot achieve single fiber dispersion when receiving powder products;
4. Long-term storage stability : Water-based suspensions are prone to sedimentation, mildew, and viscosity drift when left standing for a long time, and high-solid systems are more difficult to store.
In response to the above industrialization pain points, our company has built a complete technical chain from raw material pretreatment, controllable dissociation, customized surface modification, concentration and dispersion to application process guidance:
· The modification scheme can be customized according to the customer's resin system (water-based acrylic, epoxy, 、PU PLA , polyolefin, etc.), and the degree of substitution, surface polarity, and zeta potential can be precisely controlled;
· The product form can be selected from native suspension, modified concentrated slurry, and modified redispersible powder. Concentrated slurry products are preferred and are suitable for conventional dispersing equipment in most coating factories;
· It provides basic characterizations such as particle size distribution, rheology curve, and contact angle test, and simultaneously provides process SOPs such as feeding sequence, dispersion speed, dispersion time, and pH window to avoid formula waste caused by customers' own exploration;
· At the mass production end, the raw material traceability, online dissociation parameter monitoring, and finished product multi-index detection system have been established to control the aspect ratio and dispersion performance fluctuations of different batches of products to ensure the stability of downstream scale-up production.
Nanocellulose is not a simple ' replacement additive ' , but a bio-based nanofunctional platform that can be reused across tracks. The industry is currently shifting from the ' basic material preparation ' stage to the stage of directional modification and scenario-based formula solutions . There are three clear development directions in the future: first, low-cost continuous preparation process to reduce CNF The unit cost of 、CNC has spread to general coatings and packaging materials; second, multi-functional integrated modification, grafting hydrophobic groups, anti-corrosion groups, and UV-absorbing groups on the surface of cellulose at the same time, achieving a single filler with multiple functions of reinforcement , anti - corrosion , and aging resistance; third, collaborative development of a full bio-based system, matched with degradable resins and bio-based additives, to create a full-chain low-carbon material solution to meet higher requirements such as export product carbon footprint, degradable certification, food contact compliance, etc.
In the wave of green transformation of global materials, nanocellulose provides a new route for the coating and polymer composite industries that is different from traditional inorganic fillers and petroleum-based additives. We continue to focus on the interface modification and dispersion engineering technology of nanocellulose, and provide sample testing, joint formula development, and customized mass production supply services to coatings and new material R&D companies to help downstream customers achieve product differentiation and low-carbon upgrades.
R&D teams in the fields of coatings, polymer materials, and degradable materials are welcome to connect with technical leaders and request product technical data sheets, samples, and application test plans.
Our company can provide nanocellulose aqueous dispersions of different specifications, provide sample testing and formula adaptation technical support to formula R&D engineers, and can assist in testing emulsion system stability evaluation, hot and cold cycles, centrifugal acceleration testing, particle size characterization and other tests. R&D teams in the daily chemical and food industries are welcome to contact us to jointly develop Pickering emulsification systems and polish customized solutions.